Original paperSourceNo author review
Make your paper interactiveCreate

Text from the interactive explanation

Thin-film lithium tantalate for ultraviolet integrated electro-optic modulator

Chupao Lin, Patrick Nenezic, Arno Moerman, Simone Cammarata, Simone Atzeni, Konstantinos Akritidis, Tom Vanackere, Margot Niels, Valeria Bonito Oliva, Valeria Bonito Oliva, Xin Liang Yin, Maximilien Billet, Bart Kuyken

Nature Communications · Article in Press · 27 October 2026

Quantum computers built from trapped ions, ultra-precise atomic clocks and “solar-blind” communication links all depend on ultraviolet light that must be switched and shaped billions of times per second. Today that job falls to bulky crystals driven by kilovolts. Could it shrink onto a chip and run on a few volts?

Illustrative model The data stream switches between 0 V (bright, a “1”) and 4.2 V (dark, a “0”). The two arms are pushed in opposite directions by the electric field (amber arrows). Waves are drawn far larger and slower than reality — real UV light oscillates about 800 trillion times per second. Drag across the chip or use the slider to take control.

The speed problem

Ultraviolet (UV) light has wavelengths just shorter than violet, beyond what our eyes see. It does jobs no other light can. Ytterbium ions — leading building blocks for quantum computers and atomic clocks — respond to UV light at 369.5 nanometres. Near-UV light travels well through water, and deep-UV links are called solar-blind because sunlight at those wavelengths barely reaches the ground, leaving a dark background for signals.

Using light like this means controlling it with electronics: a modulator changes the light whenever an electrical signal arrives. For infrared telecom light, chips have done this at tens of gigahertz (billions of cycles per second) for years. For UV, the toolbox is thin:

Silicon and silicon nitride chips absorb UV.

Alumina chips guide UV well but cannot respond to voltage directly; they switch light by heating (tens of kilohertz) or by vibrating (tens of megahertz).

Bulk crystals such as BBO and KDP need kilovolts; the power needed to drive them fast heats them, capping them around 100 MHz. Bulk lithium niobate does better, but is often heat-limited near 160 MHz and can only take low UV power densities.

Trapped-ion qubits & clocks

Addressing the two hyperfine levels of a 171Yb+ ion at 369.5 nm calls for phase modulation at 12.6 GHz .

UV communication

Wireless, underwater and solar-blind UV links aim for data rates beyond 100 GHz .

UV frequency combs

Spectroscopy with combs of UV laser lines spaced from tens of MHz to tens of GHz .

The blinking race

Every lane receives the same on–off signal. Raise the signal frequency and watch which technologies can still blink. (Blinking is slowed to a viewable pace; its depth shows how much of the signal survives.)

We need a material that answers to voltage directly, at electronic speed, and survives UV light — patterned on a chip.

Meet the chip

The team at Ghent University – imec carved their modulator into a film of lithium tantalate (LiTaO3) only 300 nanometres thick — a few hundred times thinner than a human hair — resting on an insulating layer. Light is guided in a narrow ridge called a waveguide , etched 100 nm into the film.

The whole device is 1.16 mm long. Its active part, where three gold electrodes (ground–signal–ground) flank the two light paths, is just 200 µm .

Short wavelengths are unforgiving: scattering from rough surfaces grows as 1/λ4, so UV light at 375 nm scatters about 290 times more than telecom light at 1550 nm. A wet-chemical etch left the waveguide walls smooth to 0.2 nm (root-mean-square) — roughly the size of a single atom.

Why tantalate, not niobate?

Its cousin lithium niobate powers today's telecom modulators, but intense short-wavelength light makes niobate's refractive index drift (the photorefractive effect). Lithium tantalate keeps a comparably strong response to voltage while:

staying transparent down to 275 nm ;

showing a photorefractive index change below 10−6 , versus 1.4 × 10−5 for thin-film niobate (532 nm, 13 kW/cm²);

changing about 10× less with temperature .

Values cited in the paper's introduction from earlier studies.

Images cropped from Lin et al., Nat. Commun. (2026), Figs. 2–4, CC BY 4.0.

A crystal that listens to voltage

Light slows down inside any transparent material; the slowdown factor is called the refractive index . In crystals like lithium tantalate, an electric field nudges that index up or down — the Pockels effect . The response is effectively instant: no heating, no moving parts. That is what makes gigahertz switching possible.

The change is tiny. At 4.2 V, each arm's index shifts by only about 0.0005 . But a light wave counts its own crests: over 200 µm, the slowed wave falls behind by a quarter of a wavelength.

Δφ = 2π · L · Δn / λ

Look at the λ underneath: the shorter the wavelength, the bigger the phase shift from the same index change. UV light gets more effect per micrometre — one reason this electrode can be so short. Switch to telecom infrared to compare.

One arm, one electrode

A quarter-wave delay is invisible to a detector — light is still light. To turn delay into on/off, we need interference.

Turning a delay into darkness

The chip is a Mach–Zehnder interferometer : split the light into two arms, delay one relative to the other, then recombine. Where crests meet crests, the light adds up. Where crests meet troughs, it cancels and the light is thrown out of the waveguide instead.

Predict: one arm now lags the other by exactly half a wavelength . What comes out?

The electrodes are arranged ground–signal–ground , so the field points one way across the upper arm and the opposite way across the lower arm (the amber arrows in the hero). One arm speeds up while the other slows down — a push-pull design that doubles the delay and halves the voltage needed.

Two arms, one output

The voltage that turns bright into dark is the half-wave voltage, Vπ . Let's measure it the way the authors did.

Measure Vπ yourself

The authors sent a 375 nm laser through the chip and swept the voltage back and forth with a fast triangle wave repeating 400,000 times per second with a 10-volt swing. Sweeping fast avoids slow drifts from heating and stray charge. On an oscilloscope, the light rises and falls as the voltage climbs.

Your task: put one cursor on a bright peak and the other on the next dark dip along the rising ramp. The voltage difference between them is Vπ.

Why voltage × length? A longer electrode needs less voltage, so the product VπL lets devices of different sizes be compared fairly. Lower is better.

Oscilloscope · 400 kHz triangle drive

How dark is “off”?

A slow sweep from 0 to 10 V gives the full brightness curve. The extinction ratio compares the brightest and darkest points: here 22.7 dB . Decibels count factors of ten — every 10 dB is ×10 — so 22.7 dB means “off” is about 190 times dimmer than “on”. Over six devices the authors measured 19.4 ± 3.8 dB.

Notice the real chip is not perfectly balanced at 0 V: its darkest point sits near 3 V. Real interferometers rarely sit exactly balanced; in use, a steady bias voltage sets the operating point.

Slow sweep at 375 nm

The gap dilemma

The same voltage across a narrower gap makes a stronger electric field, so pulling the gold electrodes closer to the waveguide lowers VπL. But light is not perfectly confined to the ridge — its edges spill sideways. Bring the gold too close and the metal starts absorbing the light .

Challenge (our game rule): find a gap where the drive stays under 5 V and the gold steals less than 0.01 dB of light along the 200 µm electrode.

Cross-section through the electrodes

How fast can it blink?

A modulator's bandwidth is how fast it can follow a signal. Engineers quote the 3-dB bandwidth : the frequency at which the on/off signal coming out has fallen to half its low-frequency power.

Long modulators face a race. The electrical signal travels along the electrode while the light travels through the waveguide; if their speeds differ, the light drifts out of step with the voltage and the effect washes out. Here the microwave index (≈2.3) and the light's group index (≈2.8) are close — and over just 200 µm they cannot drift apart. The authors call this electrode “lumped”: short enough to act all at once.

Walk-off race

What was measured

The team drove the chip with microwaves while a fast photodetector turned the UV light back into an electrical signal — an electrical-to-optical-to-electrical (EOE) measurement. Detectors have speed limits of their own, so the authors removed the detector's response from the data (de-embedding).

Result: the response stays within 3 dB all the way to 40 GHz , the limit of their equipment. The true bandwidth may be higher; it could not be pinned down because the detector, calibrated mainly for infrared light, was the bottleneck.

Electrical measurements of the electrodes alone reach 67 GHz with only 2 dB of microwave loss. From them, the authors estimate the modulator's own roll-off at about 1 dB at 67 GHz.

Frequency response

measured EOE (Fig. 4g) estimated intrinsic EOE (Fig. 5f) measured electrical S21 of the electrodes (Fig. 5c)

The blinking race, rematch

The fifth lane is now driven by the chip's measured response (to 40 GHz) and the authors' estimate beyond it (drawn hatched).

Where it lands

Two numbers summarise a modulator: how fast it is (bandwidth) and how efficient it is (VπL, lower is better). The best place on this map is the top-left corner.

Measured as bandwidth divided by VπL, the authors report a two-orders-of-magnitude improvement over bulk lithium niobate modulators and a five-orders-of-magnitude improvement over traditional BBO/KDP crystal modulators.

Tap a point to see what it is.

This work: VπL = 0.085 V·cm at 375 nm; bandwidth above 40 GHz.

Bandwidth vs VπL, UV modulators

Efficiency across the UV–visible

Light budget: why short is good in the UV

UV waveguides lose light quickly — 7.2 dB per centimetre at 375 nm — but this device is only 1.16 mm long. Stretch it and see.

Measured on-chip loss

Light lost inside the modulator: 2.8 ± 0.6 dB , compared with a predicted 1.3 dB; the authors suggest electrode misalignment and coupling variations as likely reasons.

Getting light in and out

Coupling from fibre to chip currently costs 9.7 ± 0.3 dB per facet . Spot-size converters, already shown on other platforms, are the natural next step.

Standing up to UV

No darkening was seen with 700 µW squeezed into a 0.14 µm² mode — about 5 kW/mm² — for 5 minutes. Long-term high-power tests are planned.

Back to the ions

Remember the opening question. A ytterbium ion has two closely spaced ground levels, 12.6 GHz apart. A modulator that wiggles a UV laser's phase at frequency f adds sidebands — copies of the laser line shifted by ±f. Tune f to 12.6 GHz and one laser can reach both levels.

Bulk crystals can do this today, at kilovolt-scale drive and lab-bench size. The chip in this paper switched UV light with 4.2 V and kept its response to beyond 40 GHz.

Tune the sidebands

“These results enable the transition from lab-scale bulk optical setups to robust, chip-scale systems, including on-chip trapped-ion quantum computing, portable atomic clocks, UV spectroscopy, and high-bandwidth solar-blind UV communications.” — Lin et al., 2026

What comes next, according to the authors

Cut fibre-to-chip coupling loss with spot-size converters.

Lower waveguide loss with oxygen annealing (520 °C), a silica top cladding and smoother etching.

Terminate the electrodes with a matched 23 Ω load to avoid reflections.

Build longer “travelling-wave” modulators for UV frequency combs — helped by the closely matched microwave and optical speeds.

Combine lithium tantalate with ultra-low-loss alumina UV chips by micro-transfer printing.

Test stability under high-power UV over long periods.

Source & credits

Chupao Lin, Patrick Nenezic, Arno Moerman, Simone Cammarata, Simone Atzeni, Konstantinos Akritidis, Tom Vanackere, Margot Niels, He Li, Valeria Bonito Oliva, Xin Yin, Maximilien Billet & Bart Kuyken. “Thin-film lithium tantalate for ultraviolet integrated electro-optic modulator.” Nature Communications (2026), Article in Press. https://doi.org/10.1038/s41467-026-78862-6

Version. This guide follows the Article in Press published on 27 October 2026 (received 28 May 2026, accepted 6 October 2026) — the peer-reviewed accepted manuscript, which the final edited version will later replace. An earlier version appeared as the preprint arXiv:2605.02758v1 (4 May 2026). During peer review the authors added new high-speed measurements, so the preprint's detector-limited 922 MHz bandwidth is superseded by the published result of more than 40 GHz.

Research. Photonics Research Group and IDLab, Department of Information Technology (INTEC), Ghent University – imec, Ghent, Belgium. Supported by the Horizon Europe project Qu-PIC (101135845).

Licence and adaptations. Article © The Author(s) 2026, published under a Creative Commons Attribution 4.0 International licence. Photographs and micrographs are cropped from Figs. 2–4. Measured curves were digitized from Figs. 4–6 and redrawn; simulated and estimated curves are labelled as such. Interactive scenes marked “Illustrative model” are teaching models built from the paper's reported values, not reproductions of its data.

Topics in this iPaper

Physics
Precise manipulation of ultraviolet (UV) and visible light is fundamental to a diverse range of emerging technologies

Introduction, page 1 (Article in Press); page 2 (arXiv preprint)

Engineering
The electrodes are produced by a lift-off process.

Methods, Fabrication, page 8 (Article in Press); page 14 (arXiv preprint)

electro optic modulator
we demonstrate a high-performance integrated modulator based on a TFLT platform operating in the UV

Introduction, page 3 (Article in Press); page 4 (arXiv preprint)

lithium tantalate
thin-film lithium tantalate (TFLT) presents a compelling alternative for UV applications

Introduction, page 2 (Article in Press); page 4 (arXiv preprint)

integrated photonics
Shifting toward an integrated photonic platform

Introduction, page 1 (Article in Press); page 2 (arXiv preprint)

pockels effect
A Pockels coefficient r33 of 35 pm/V is used in the simulation

Results, Electro-optical performance, page 5 (Article in Press); page 10 (arXiv preprint)

mach zehnder interferometer
we employ an MZI architecture to ensure operational robustness

Results, Device design and implementation, page 3 (Article in Press); page 4 (arXiv preprint)

ultraviolet photonics
Realizing high-speed UV modulation remains a challenge

Introduction, page 1 (Article in Press); page 2 (arXiv preprint)