Original paperSourceNo author review
Make your paper interactiveCreate

Text from the interactive explanation

Multi-model collaborative early warning for battery systems with integrated fiber optic sensors

Jiangong Zhu, Chao Yu, Yi Jiang, Wolfgang Schade, Martin Angelmahr, Xuezhe Wei, Haifeng Dai

Battery safety · fiber-optic sensing

Watch the top-left corner: one heated cell, 128 fiber readings.

An electric-car pack holds hundreds of cells, yet a car’s battery management system (BMS) typically watches temperature at only a few dozen spots. The researchers threaded light-carrying fibers through packs — in a car pack, 32 temperature points became 540 — and let four simple rules read the pattern together. In the recorded failures they report, the alarm came up to 706 s earlier in the lab and 554 s earlier in a real car than the conventional voltage-based alarm.

Above: the lab module during an overheating test, replayed from the recorded fiber temperatures at 30× speed. The heated cell (dashed ring) was already about 70 °C when the record starts. A few seconds around 46–60 s show brief spikes on the top fiber; from about 470 s that fiber gives no valid readings; runaway spreads after about 750 s and more fibers stop reporting. Sensor mapping: our reading of the data order.

What are we trying to catch?

A lithium-ion cell packs a lot of energy into a small can. In thermal runaway , a cell starts heating itself faster than it can shed that heat: warmth speeds up reactions inside, the reactions release more heat, and the loop feeds itself. A runaway cell can vent and burn — and pass enough heat to its neighbours to set them off too.

Where does trouble begin? The anode in each cell is covered by a thin protective layer (the SEI, solid electrolyte interphase). Its initial breakdown typically starts at 80–120 °C , with a peak around 100 °C. In the authors’ calorimeter tests (accelerating-rate calorimetry, ARC) of fresh cells, self-heating began at about 110–155 °C — and this onset is expected to fall as batteries age. So the first warning rule uses 100 °C .

At 100 % charge, self-heating began at 115 °C — 15 °C above the warning threshold.

Fuller cells are less stable — the fuller the charge, the lower the temperature at which self-heating began. But a thermometer only helps if it sits near the cell that is heating.

A thermometer made of light

The sensors are fiber Bragg gratings (FBGs) . Start with a thin glass fiber that carries light. A femtosecond laser writes tiny striped patterns — gratings — into it. Each grating reflects one narrow colour of light and lets the rest pass. Warm a grating and its stripes stretch, so the reflected colour shifts: by about 11 picometres per °C in the authors’ calibration. Many gratings on one fiber, each tuned to its own colour, make many thermometers on one wire.

Grating 7 at 120 °C → reflected peak shifted by ≈1.10 nm (100 °C × 11 pm/°C) relative to 20 °C.

From one fiber to a whole car

One dot per sensing point in the car pack (REPORTED counts); arrangement is illustrative.

What would a few thermometers have seen?

With only 8 thermometers spread evenly, when would any of them first read above 100 °C?

Your 8 points

Trouble that starts in one cell is local. With dense fibers, the grating touching the heated cell crossed 100 °C within the first minute of the record. Thin out the sensors and that one reading is easily missed: the next readings above 100 °C arrive only after about 750 s, when runaway is already spreading. This is the paper’s motivation — and in their tests, the same warning rules fed with sparse BMS data warned later or missed altogether (section 05).

First-crossing times are COMPUTED HERE from the measured record for the points you keep, ignoring points with no valid reading. In several seconds between 46 and 60 s, every reporting grating on the top fiber — even those far from the heated cell — read 211–457 °C at once; the checkbox above leaves those seconds out of the count, and you can switch that off to see them counted.

Four rules, any one raises the alarm

REPORTED Thresholds as reported for the dense fiber data; the boundary in rule ③ was fitted separately for the module and the pack. The four rules run in parallel, and any single one triggers the warning.

Why not just watch heating speed?

The authors measured the fastest surface heating rate in 18 single-cell tests. Fast heating is not always danger: normal fast cycling (#18, 0.25 °C/s) heated faster than slow overcharging (#12 at 0.036 and #13 at 0.199 °C/s) and faster than every overdischarging test (0.050–0.200 °C/s). Slow overcharging stayed far below 1 °C/s.

So heat rate alone cannot tell danger from hard work. The fix: also measure the pattern of temperatures across the pack.

Build a temperature pattern: the entropy sandbox

Shannon entropy measures how spread out a set of values is. Sort every sensing point’s temperature rise into 1 °C bins: if they all land in a few bins, entropy is low; if they scatter across many bins, it is high. Ordinary warming raises entropy a little, in a predictable way. The authors drew a boundary above normal behaviour: a pattern more uneven than expected for its average warming crosses it.

Sandbox: ΔT = warm + (j − 0.5)·(0.6·warm + 0.8) + hot·exp(−(d/r)²), with j a fixed pseudo-random number per point and d the distance (grid steps) from the hot-spot centre; absolute temperature assumes 25 °C ambient. Entropy SE = −Σ pᵢ log₂ pᵢ over 1 °C bins from floor(min) to ceil(max). Boundary SEB(x) = a·e−b·x + c + Etol with the lab-module values a = −3.352, b = 0.08545, c = 4.418, Etol = 0.3 (Supplementary Table 4). Grey cloud: measured normal charge/discharge of the lab module at 0, 25 and 40 °C ambient (Fig. 3e Source Data, subsampled). In the paper, entropy is computed on temperature changes since the start of each recording segment, only while the module’s average temperature is trending upward; rule ④ uses the entropy’s rate of change.

Replay the four failures on their own clocks

Four recorded failures, each on the clock times printed in the paper: two lab-module tests and two real cars. Pick a comparison. Same rules, different eyes keeps the warning framework fixed and swaps its input — sparse BMS readings or dense fiber readings. Same eyes, different rules feeds everyone the same fiber data and compares four warning methods.

The conventional BMS alarm fires when a parallel-cell voltage changes by ≥ 1 V/s. With sparse input the same temperature thresholds (100 °C, 1 °C/s) were used; the entropy boundary was refitted for the sparse data and its rate threshold is 0.2 (Supplementary Table 3). The comparison methods: composite threshold — alarm when the hottest point is ≥ 100 °C and either heating is ≥ 0.2 °C/s or the hottest–coolest gap is ≥ 20 °C; variance + LOI — alarm when temperatures are widely scattered (variance ≥ 50) and the hottest 10 % cluster tightly around the hot spot (LOI ≤ 0.2); CUSUM — adds up each sensor’s unusual upward drift and alarms when the running sum passes a limit. The authors calibrated all three on normal operating data to suppress false alarms (Supplementary Note 4).

Warning is not intervention.

These are the times when an alarm would have been raised in recorded data, analysed afterwards. The paper does not test what a driver or the battery system does next, or whether a runaway could be stopped. The conclusions apply to these four recorded failures.

What the measurements show

Could it ride in every car?

The authors estimate what an onboard version would need. This is an estimate, not yet run on car hardware — they list that as future work.

What this does not show yet

Few failures. Two lab modules and two cars with runaway, with a limited variety of failure modes.

Untested failure types. Internal short circuits, mechanical damage and other complex failures still need validation.

Other batteries. Effects of aging, other cell chemistries (the tests used NCM/graphite 18650 cells) and other pack designs on the entropy model have not been systematically evaluated.

Tuned per system. Parameters were fitted separately for the module and the pack; the authors propose a parameter library updated over the air as future work.

One yardstick. Lead times are measured against the voltage-based BMS alarm only — and Vehicle 4’s margin was 25 s.

Back to the question

Could a pack warn us minutes before it fails?

In these recorded cases, yes: dense fiber sensing plus four cooperating rules raised the alarm 706 s (lab overheating) and 554 s (Vehicle 1) before the conventional voltage alarm, and never later than it in the four failures. What the extra minutes are used for — and whether this holds across more batteries — is the next question.

Sources and provenance

Zhu, J., Yu, C., Jiang, Y., Schade, W., Angelmahr, M., Wei, X. & Dai, H. “Multi-model collaborative early warning for battery systems with integrated fiber optic sensors.” Nature Communications 17, 10700 (2026). https://doi.org/10.1038/s41467-026-78461-5

Open access under CC BY 4.0 (https://creativecommons.org/licenses/by/4.0/).

All visuals are original redrawings. Measured temperatures, Fig. 3 and Fig. 5 values: Source Data file of the article (CC BY 4.0) — subsampled and redrawn; alarm times: Tables 1–2; parameters and benchmark descriptions: Supplementary Information. Changes: redrawn, rescaled, recoloured, combined with explanatory text.

Authors’ code: github.com/yuchao210/Multi-model-collaborative-early-warning-for-battery-systems-with-integrated-fiber-optic-sensors · Data: https://doi.org/10.5281/zenodo.22121425

Topics in this iPaper

Engineering
An integrated sensing scheme increases temperature sensing points within the battery pack from 32 to 540 with minimal wiring complexity and is validated in real-world vehicle operation.

Abstract, page 1

thermal runaway
Compared with conventional BMS warning benchmarks, the framework provides maximum warning lead times of 706 s in laboratory modules and 554 s in real-world vehicle operation.

Abstract, page 1

lithium ion batteries
Lithium-ion batteries (LIBs) are currently among the most widely used clean energy storage devices

Introduction, page 1

fiber bragg gratings
this study employs fiber optic sensors assembled from femtosecond-laser-inscribed Fiber Bragg Gratings (FBGs) to achieve distributed temperature sensing within the battery system

Introduction, page 4

battery management systems
The safety assessment of battery systems is constrained by sparse temperature measurements and monolithic diagnostic frameworks in conventional battery management systems (BMS).

Abstract, page 1

shannon entropy
We establish a functional relationship between temperature Shannon entropy (SE) and average temperature variation to derive a dynamic warning boundary

Abstract, page 1

electric vehicles
seven EVs are selected in this study and labeled as “Vehicle 1” through “Vehicle 7”

Results, page 4