Original paperSourceNo author review
Make your paper interactiveCreate

Text from the interactive explanation

Comparative Analysis via CFD Simulation on the Impact of Graphite Anode Morphologies on the Discharge of a Lithium-Ion Battery

Alessio Lombardo Lombardo Pontillo, Agnese Marcato, Daniele Versaci, Daniele Luca Marchisio, Gianluca Boccardo

Flakes, not marbles

A battery’s charge meter shows one number. Inside its graphite electrode, the lithium behind that number can be spread evenly — or crowded against one side. A 2025 simulation study shows that which picture a model paints depends on a detail models often simplify: the shape of the graphite grains.

Here, three digital electrodes fill with lithium at the same current. Change the speed and watch their insides part ways.

Which of these interiors is closest to a real battery? By the end of the tour you will be able to answer — and see what the researchers found.

Fill 35% · C/3

The grains are flakes, not marbles

Before asking where the lithium goes, meet the material it goes into.

A lithium-ion battery has two electrodes. In many cells, one of them is a layer of graphite grains glued onto copper foil and soaked in a liquid electrolyte that carries lithium ions (Li⁺). Graphite is carbon arranged in stacked sheets, and lithium can slip in between those sheets — a process called intercalation .

In this study the graphite layer was about 60 µm thick, roughly the width of a human hair. It was tested in a half cell , facing a disc of lithium metal. In a half cell, “discharge” means lithium flowing out of the metal and into the graphite, gradually filling it. That is the filling you watched above.

FESEM images from Figure 1 of Lombardo Pontillo et al. (2025), CC BY 4.0; cropped.

Yet a widely used family of battery models — the pseudo-2D, or Doyle–Fuller–Newman, approach — treats every grain as a sphere of the same size. The authors point out that this is acceptable for some cathode materials, but graphite’s layered structure makes its grains flat : one dimension much smaller than the other two.

Squash a sphere of radius 8 µm into the flattened ellipsoid that fits inside it — the same move the paper’s workflow makes. Semi-axes a > b ≫ c, with the half-thickness c fixed at 1.5 µm as in the paper; the a/b ratio of 1.3 is an illustrative choice. Numbers are computed geometry.

Two things change at once. A flake is thin, so lithium has only a short trip from its surface to its centre. And flakes lie flat, like fallen leaves, which can block the liquid paths between them. Which effect wins inside a working electrode? To find out, you need an electrode made of flakes.

Build a digital electrode

The authors wrote an automated, open workflow that turns microscope measurements into a 3D digital twin of the electrode. Run it yourself, in miniature.

IllustrativeA 2D animation of the idea. The paper performed these steps in 3D with Yade (discrete element method), Blender’s physics engine and a Java script driving COMSOL Multiphysics 6.1. Grain sizes are drawn from the paper’s measured size distribution.

What the paper measured on its three 3D electrodes

The green band is the measured porosity of the real electrode (0.300, with an experimental error of roughly 10%). Porosity is the fraction of the electrode filled by liquid. Tortuosity measures how winding the liquid paths are compared with a straight channel; the authors computed it with the TauFactor algorithm in the direction from separator to copper.

Porosity can’t tell flakes from mixed spheres — both land in the measured range, while identical spheres leave too much empty space. Tortuosity can: 7.8 for the flake electrode versus about 2 for both sphere electrodes. What does a tortuosity of 7.8 feel like to an ion?

A maze for ions

Lithium ions arrive from the separator at the top and must travel through the liquid between the grains. Race them.

IllustrativeIons take random steps with a gentle push towards the copper, and cannot pass through grains. Tap a column to drop a traced ion there. These are 2D slices: in 3D, ions can also slip around a grain sideways, so the slice exaggerates the maze.

Predict first: which electrode slows the ions most?

Table 2 of the paper. Higher = more hindered transport through the liquid.

Flat-lying flakes act like overlapping roof tiles. Ions have to find the gaps and zig-zag sideways, so fewer of them reach the deep layers near the copper in a given time. Keep this in mind — it is the first of two bottlenecks.

Getting inside a grain

Reaching a grain is only half the trip. Lithium then has to creep inwards through solid graphite — the second bottleneck.

Inside a grain, lithium spreads by diffusion , and in solid graphite that is slow. The paper measured an average diffusion coefficient of D = 1.317 × 10⁻¹⁴ m²/s with a pulsed lab test (GITT). A handy rule of thumb: diffusing a distance ℓ takes about ℓ²/D.

Flake, half-thickness 1.5 µm: ≈ 3 min

Small sphere, radius 2 µm: ≈ 5 min

Big sphere, radius 6 µm: ≈ 46 min

Compare those with the length of a discharge: 10 hours at C/10, but only 1 hour at 1C. The C-rate says how fast the battery is charged or discharged: C/10 completes in 10 hours, 1C in one hour.

On the right, lithium enters each grain through its surface at a steady rate. Change the speed and watch the centres.

Graphs under each grain: filling from centre to surface, in percentage points above or below that grain’s average.

Computed hereA one-dimensional diffusion calculation (Fick’s law) using the paper’s diffusion coefficient, with a constant inward flux. It is not the paper’s full electrochemical model, which also solves the electrolyte, electric potentials and surface reactions.

The GITT test applies short current pulses at C/20 and watches the voltage relax. From each pulse the team extracted a diffusion coefficient. It swings over several orders of magnitude as the graphite fills; for speed, the simulations used one constant average value (the flat line). Their code can also take a value that changes with the state of charge.

MeasuredInterpolated GITT data from the authors’ public dataset (Zenodo, CC BY 4.0), as in the paper’s Figure 3c.

Two bottlenecks, two shapes. Flakes are thin, so lithium gets inside them easily — but they make it hard to get between them. Big spheres leave open paths between grains, but their cores fill late. Now predict what that does to a whole electrode.

Put it together: the lithium tide

The paper compared its three electrodes when they were exactly half full (state of charge 50%), at four speeds. Predict, explore, then compare with the real simulation maps.

IllustrativeLeft: the teaching model. Its vertical spread grows with speed × (tortuosity ÷ porosity) from the paper’s Table 2; the lag inside each grain grows with (grain size)² × speed ÷ D. Its constants were tuned to echo the paper’s Figure 7 — it does not solve the paper’s equations.

At 1C, which electrode piles lithium up near the separator?

Which one shows grains with lagging (blue) cores?

Make your predictions, then reveal what the paper’s 3D simulations show.

Paper resultFigure 7 of Lombardo Pontillo et al. (2025), CC BY 4.0; rotated. Local intercalated lithium (cs/cs,max, 0.38 blue → 0.57 red) at 50% state of charge. Columns: ellipsoids, polydispersed spheres, monodispersed spheres. Highlighted row: 1C.

Same total lithium, three different interiors. In the paper’s simulations the flake electrode develops a strong top-to-bottom gradient as the speed rises, with almost no gradient inside each thin flake. Mixed spheres show lagging cores in their biggest grains. Identical spheres stay nearly uniform until 1C. The authors trace the vertical gradient to the flake electrode’s higher tortuosity — and note that such vertical gradients are widely observed with X-ray analysis of real electrodes.

What the voltage can — and can’t — tell you

From outside, you can only watch the voltage. Here are the paper’s actual discharge curves, simulated and measured.

Figure 6a of Lombardo Pontillo et al. (2025), CC BY 4.0; cropped, legend repositioned. Axes: state of charge (log) vs cell voltage in volts (log). The public dataset does not include the 1C numbers, so this panel is shown as published.

Paper dataSimulated curves from the paper’s 3D COMSOL simulations and the measured C/10 half-cell curve, from the authors’ public dataset (Zenodo, CC BY 4.0), downsampled. As in the paper, voltage is graphite versus lithium metal.

As graphite fills, its voltage against lithium metal drops from about 2 V to nearly zero. The curve has steps : places where the slope changes as lithium reorganises inside graphite into different stages. The authors plot both axes on logarithmic scales to make those stages visible.

At C/10, which simulated electrode is closest to the lab measurement?

Pick one to see how close each simulation came.

At C/10 the three simulations reproduce the measurement reasonably well, and the differences in error are moderate. The authors read this as a sign that the three digital electrodes are comparable, and that at low current, grain shape barely shows up in the voltage.

Speed things up and the curves start to separate — mostly near the steps. At 1C the differences are largest: the identical-sphere curve also departs from the flakes, especially near the end of discharge.

The voltage alone hides most of the story. At gentle currents, three very different interiors produce nearly the same curve. Only by looking inside — as the 3D simulations do — do the differences in local lithium become visible.

Why the inside matters

Back to the opening question: half full — but where? The answer depends on the grains, and the answer matters for how batteries age.

The processes that slowly wear a battery out happen locally . One example is the solid electrolyte interphase (SEI) , a thin layer that grows where electrode meets electrolyte. The authors argue that because such irreversible processes depend on local concentrations, only models with a realistic electrode geometry can describe them accurately — and they name SEI formation as the focus of their next work.

Their conclusion: geometry shapes how grains are arranged, the porosity and the reactive surface area. That changes how ions are distributed and so how fast reactions run at each spot, even when the current is uniform. Spherical-grain models give more uniform transport and a flatter lithium profile; flake-shaped grains do not.

What this work brings closer is a reproducible, open workflow : swap in different particle shapes, size distributions or material properties, and test on the computer what an electrode will do — helping, in the authors’ words, to optimise material preparation and processing conditions.

What the model leaves out (for now)

Grains are smooth ellipsoids with a fixed thickness; real graphite is rough and irregular.

No SEI growth, lithium plating or other ageing reactions.

No heat, and no grain movement or cracking during cycling.

One average diffusion coefficient instead of a filling-dependent one.

Open science

Geometry code: mulmopro/yade-ellipsoids. Simulation set-up for COMSOL: mulmopro/battery_porescale (both GPL-3.0). Input, experimental and simulation data: Zenodo record 14931656 (CC BY 4.0).

Source & credits

Lombardo Pontillo, A.; Marcato, A.; Versaci, D.; Marchisio, D.; Boccardo, G. “Comparative Analysis via CFD Simulation on the Impact of Graphite Anode Morphologies on the Discharge of a Lithium-Ion Battery.” Batteries 2025 , 11(7), 252. https://doi.org/10.3390/batteries11070252

Published 2 July 2025 by MDPI under a Creative Commons Attribution 4.0 licence. The text read for this guide is the published article as deposited in the Politecnico di Torino institutional repository (IRIS, handle 11583/3003552).

Research team and project

Department of Applied Science and Technology, Politecnico di Torino, Italy (all authors); Agnese Marcato also at Los Alamos National Laboratory, USA. Funded by the European research initiative Battery 2030+ (grant agreement 957213), the BIG-MAP project — Battery Interface Genome–Materials Acceleration Platform (grant agreement 957189), the Horizon Europe project BatCat (grant agreement 101137725), and ICSC – Centro Nazionale di Ricerca in High Performance Computing, Big Data and Quantum Computing (NextGenerationEU).

What is measured, simulated or illustrative here

MeasuredMicroscope images, grain size distribution, porosity 0.300, the C/10 lab discharge curve and the GITT diffusion data (authors’ lab).

Paper resultTable 2 geometry values, the simulated discharge curves (Figures 5–6, dataset), RMSE values and the concentration maps of Figure 7, all from the authors’ 3D COMSOL simulations.

IllustrativeThe animated electrodes, ion races, packing animation and lithium-tide colours are teaching models built for this guide; they do not reproduce the paper’s simulations. The single-grain diffusion panel is a simple calculation using the paper’s diffusion coefficient.

Figures, data and fonts

Figures 1, 6 and 7 are reproduced from the article under CC BY 4.0 (Figure 1 cropped into panels; Figure 6 panel (a) cropped with its legend repositioned; Figure 7 rotated). Discharge curves, particle size distribution and diffusion data come from the authors’ Zenodo dataset (CC BY 4.0), downsampled for display. Colour scale: Turbo colormap (Google, Apache 2.0). Fonts: Space Grotesk, Inter and JetBrains Mono (SIL Open Font License).

An interactive companion by iPaper.ai (https://ipaper.ai).

Topics in this iPaper

Engineering
we present a computational workflow that overcomes these limitations by incorporating a more realistic representation of graphite morphologies

Abstract, page 1

Chemistry
The micro-scale 3D modeling of LiBs is centered on the local numerical resolution of the charge and mass conservation of intercalated lithium and lithium ion

Section 2 (Governing Equations), page 4

lithium ion batteries
Keywords: battery modeling; lithium-ion batteries; CFD; electrode morphologies; COMSOL

Keywords, page 1

graphite anodes
graphite anodes cannot be modeled under this assumption

Section 1 (Introduction), page 2

electrode microstructure
three different electrodes of increasing geometric complexity: one with monodispersed spheres, one with polydispersed spheres, and one with polydispersed ellipsoids

Section 1 (Introduction), page 3

computational fluid dynamics
Comparative Analysis via CFD Simulation on the Impact of Graphite Anode Morphologies

Title and Keywords, page 1

discrete element method
Electrodes have been recreated by Discrete Element Method (DEM) simulations using the periodic compression routine implemented in the open-source code Yade

Section 3.2, page 9

tortuosity
caused by the increased tortuosity within the electrodes, which is effectively higher for configurations with ellipsoidal particles

Section 4, page 16